Tuesday, November 21, 2017

Re: [MW:27031] WPS REG

One Test Coupon 20mm thk & other test coupon 10mm 

20mm coupon carry out all test including Impact Test (Qualification range is 16 to 40mm)

10mm coupon : carry out only impact Test...to get qualification range 10 to 40mm;  to cover shell thicknerss 14.27mm

regards

Aly

Virus-free. www.avast.com

On Sat, Nov 18, 2017 at 1:02 PM, Subrata Das <subrata19732111@gmail.com> wrote:
Dear Experts,
Please guide me for test coupon thickness to be considered for below case

- Vessel thickness 14.27mm
- Nozzle thickness 40mm
- Set in type Nozzle on Vessel shell
- Full penetration weld with fillet
- Impact test applicable
- No PWHT

Do I need to consider Nozzle thickness 40mm or Shell thickness 14.27mm. Appreciate your reply in advance with Code clauses.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...