Re: [MW:27026] Hydrogen level

Just to add, the sources of Hydrogen are Moisture, carbanaceous materials like Grease etc.. & Paint. The source of H2 in the shielding gas is moisture condensation which will not be a problem with welding grade purity Argon.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Monday, November 20, 2017, 2:27:48 PM GMT+4, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Normally for CO2 shielding gas for FCAW welding, a Heater can be fitted to the Gas cyclinder along with the Regulator and Flow meter.

Argon used in purging gas shouldn't be a problem as the gas will be heated up due to welding Heat.

I haven't comes across Hydrogen problems in GTAW welding.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Monday, November 20, 2017, 11:29:48 AM GMT+4, Mohamed Ali <marb8389@gmail.com> wrote:


Dear Experts,

Could you please tell, how can ensure no hydrogen is is the backing or Shielding gas??
if use Argon gas 99.997% during welding.




Regards,
Mohamed


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...