Saturday, November 18, 2017

Re: [MW:27009] WPS REG

Please refer to the below snap shot of ASME Sec.IX.

Inline image


In case if you have used a combination of Welding process during PQR, below section also will be useful.

Inline image




Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Saturday, November 18, 2017, 1:42:27 PM GMT+4, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:


thickness should cover both

Virus-free. www.avast.com

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sat, Nov 18, 2017 at 2:32 PM, Subrata Das <subrata19732111@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (subrata19732111@gmail.com) Add cleanup rule | More info

Dear Experts,
Please guide me for test coupon thickness to be considered for below case

- Vessel thickness 14.27mm
- Nozzle thickness 40mm
- Set in type Nozzle on Vessel shell
- Full penetration weld with fillet
- Impact test applicable
- No PWHT

Do I need to consider Nozzle thickness 40mm or Shell thickness 14.27mm. Appreciate your reply in advance with Code clauses.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...