Re: [MW:26990] PWHT of lifting lug

But I am. Surprised, how you lifted the vessel for PWHT with out lifting lugs... 

Anyways you can do welding on pad after PWHT also,  as it is not directly welded to pressure part anymore. 

But keeping consideration of thickness heating and welding will involve more heat distribution... Pls take care of preheat too. 

On Nov 15, 2017 6:57 PM, "Muhammed Ibrahim PK" <ibratech@gmail.com> wrote:
Gents,

I need to clarify one issue with PWHT of a lifting lug.

An ASME Sec VIII Div I vessel require PWHT. lifting lug pad welded with vessel and PWHT done. After PWHT a lifting lug will weld with the pad. The lifting lug having thickness of 40mm and having full penetration groove weld with pad. Is this lifting lug to pad welding required PWHT ?. Please find attached drawing detail for reference.

Your valuable advice will be appreciated.

Thanks & Regards
Muhammed Ibrahim PK

Virus-free. www.avast.com

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...