[MW:27055] Crack after tack welding by using E6013 electrode

Dear Experts,

One of my customer is using our E6013 electrode which is highly cellulosic.

He has observed crack after tack welding.

Need some solution for this problem.

Thank you in advance.

Regards,

Amit Singh

--