Re: [MW:26937] preheating required for T12 material

Please see below the requirement from ASME Sec.I Power Boilers.

Inline image


I suppose PW-39 exemptions are applicable only for socket welds & seal welds. Hope some experts can throw more light on this subject.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Monday, October 23, 2017, 8:45:39 AM GMT+4, 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:


Please find below the requirement from Power Piping ASME B31.1

Inline image

Please find below the Requirement from ASME Sec.VIII Div.I

Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Monday, October 23, 2017, 6:28:03 AM GMT+4, Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:


If you do not go for SR, then you have to do preheat otherwise no. Pl ref PW39

On 23-Oct-2017 7:49 am, "'james gerald' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Both Chromium and Molybdenum increases hardenability(propensity to Brittleness) and hence required to be pre-heated.

Please follow below guidelines table.

Inline image


Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Sunday, October 22, 2017, 1:46:51 PM GMT+4, 'Sankaran Sp' via Materials & Welding <materials-welding@ googlegroups.com> wrote:


Dear Mr.Rameez,

T12 is alloy steel and it is having additional alloying elements with Cr,Mo combinations, hence pre- heating is advisable before welding.  


Regards,
Sankaran.SP

On Tuesday 10 October 2017, 8:01:14 AM IST, Rameez khan RK <rk.rameezkhan21@gmail.com> wrote:


Dear Experts,
                      can any one tell me pre-heating required for T12 material blow 6mm . This material in boiler water wall . Please tell me with standard and where i found this in ASME


THANKING YOU 

RAMEEZ  

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...