Wednesday, October 11, 2017

Re: [MW:26906] Welding procedure with Impact test

It is an supplementary essential variable ... so need to perform impact test .

With Warm Regards,

S.TAMIZH SELVAN,
Mobile: +91-9597370860 ( India )
          

On Wed, Oct 11, 2017 at 1:05 PM, Somu Meganathan <amsomu04@gmail.com> wrote:
Hello all,

Till  today we have not qualified any welding procedures with impact test requirements. Now we got an order with impact test requirements. i.e, HE body flange need to be impact tested at -9 deg. C. It seems we need to qualify the welding procedures with impact test.

My doubts are We need to qualify the welding procedure with impact with -9 Deg.C or can we do less than -9 Deg.C. Is it required impact tested welding procedures, when the materials need impact test qualified?

Regards,
M.SOMU
 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...