Re: [MW:26895] MTC Dimensions are different from Actual Dimensions - Help Pls..

This is indication that plate or MTC is not genuine.

On 9 Oct 2017 9:01 am, "Kannayeram Gnanapandithan" <kgpandithan@gmail.com> wrote:
Even though Heat nos are same, Plate nos will differ and have different properties. pl ask for original MTC

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sun, Oct 8, 2017 at 11:59 PM, Solidworks <ahsan4743@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (ahsan4743@gmail.com) Add cleanup rule | More info

Hi Experts,

I need your help. Client has been rejected plate, material is S275JR because MTC dimensions and Actual dimensions on plates are not matched. Below mentioned dimensions are,

MTC Dimensions: 25x1219x2438  - Heat No. 3073728

Actual Dimensions: 25x2000x6000 - Heat No. 3073728

I have been informed to our planning team, dimensions are not matched as per MTC and they said to us ''Heat number are different from actual plates? If same heat number, why it is rejected? Size has nothing to do with material grade''

Can someone please guide me what I need to say to our planning team.

Many thanks!

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...