Hi

I have carried out several procedures as per EN 15614 and SEC IX

The testing requirements , test coupon size all are different.

The answer to your question is NO.

Please follow your construction code.

Regards

Prem Nautiyal

PREM S NAUTIYAL
CELL : 9769316004





From: ABHISHEK SINGH <mech.abhi17@gmail.com>
Sent: Sat, 7 Oct 2017 17:42:26 GMT+0530
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:26879] Weld overlay PD5500

Dear Experts,

In my Job construction code is PD5500. Can I use Overlay  PQR qualified as per ASME Sec. IX instead of EN15614-7??

Regards
Abhishek Singh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https:roups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...