Wednesday, October 4, 2017

Re: [MW:26862] Ferrite test

Hi

Ferrite tester is available with the NDE inspection agencies, you may depute for testing. There will be an acceptance criteria for Ferrite number in the EIL specification, please refer.

Regards
P Govindan

On Oct 4, 2017 08:40, "Pankaj Kolhe" <pankaj.kolhe15@gmail.com> wrote:

Dear experts

We have pipe SA 358 tp 304 CL 1
In EIL qap ferrite test is mentioned
How to check whether this test is really required. As per SA 358 it is supplementary requirement.
How FN to be decided for acceptance.  How to calculate.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...