Hi Friend

PWHT of D/End after forming depends upon various factor and accordingly to be decided
i) Fiber elongation occurred during forming (Generally above 5% needs PWHT)
ii)Service condition i.e. Sour service required PWHT
iii) Clients spec Some of the spec allows SR and some insists for Normalising
 Accordingly  you have to decide
Regards
Hegde




On Monday, 2 October 2017 1:44 PM, udaya bhaskar <dusroni@gmail.com> wrote:


you can proceed for all thk , except 6mm. as per ASME SR is mandatory for BQ MOC.

On Tue, Sep 26, 2017 at 7:33 PM, Pankaj Kolhe <pankaj.kolhe15@gmail.com> wrote:
Dear Experts,

AS per IL spec.all cold formed heads need to be stress relieved.
we have 6mm,10mm,12mm,16mm & 20 mm thk dish end in our job.

so my question is shall i do SR for all thickness dish end or how to proceed.

MOC 516-70


pankaj
--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.



--
With Regards

Udyabahaskar.D

+919951728551
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...