Re: [MW:26856] Using ER308 for 316 pipe welding

Dear giri,

According to ASME IX & B31.3 , Can we use ER308 for welding of SS316 pipe?

ER308 electrodes uses for welding of CS to SS not for SS.
for SS316 welding you can go for 316 electrodes.
if you use SS308 electrodes for SS316 , it would crack.

On Fri, Sep 29, 2017 at 7:27 AM, gigi <anhtrangnghieng@gmail.com> wrote:

Dear experts,

 

According to ASME IX & B31.3 , Can we use ER308 for welding of SS316 pipe?

 

Thanks in advance.

 

Gigi

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
With Regards

Udyabahaskar.D

+919951728551

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...