Re: [MW:26855] Using ER308 for 316 pipe welding

Since Mo is not there, do not go for 308 instead you can use 317. Mo is very much essential for Crevice corrosion resistance. 

On 02-Oct-2017 8:44 am, "Dinesh Somwanshi" <som.din@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (som.din@gmail.com) Add cleanup rule | More info

Dear
Its better to go with equivalent or higher grade ER316, As to avaoid
precipitation hardening due to lack of chrome at weld zones.

On 9/29/17, gigi <anhtrangnghieng@gmail.com> wrote:
> Dear experts,
>
>
>
> According to ASME IX & B31.3 , Can we use ER308 for welding of SS316 pipe?
>
>
>
> Thanks in advance.
>
>
>
> Gigi
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.
>


--
*Thanks & Regards*

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER

AUTHORIZED PIPING / WELDING / NDT / PAINTING INSPECTION PERSONNEL
API 570 - Piping Inspector, AWS - CWI , CSWIP 3.1*,*BGAS  Gr 2 / 3
NDT II -UT , RT , MT , PT, VT
+7 924 374 6660 Russia , 00919881344135 India ( Whatsapp )
Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...