Tuesday, October 31, 2017

[MW:26949] Hydro cracker Unit - Heater Radial coil welding material 347H

Dears Experts,


Hydro cracker Unit, Heater Radial coil welding base material 347H and Filler wire ER347H(Metrode) Size 4' x 13.49 Thickness 

When we start the welding, getting crack in the weld stop and start point 

Please advise me


Regards,

Amul Raj T    

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...