Dear Sir,

Kindly refer Table 14 for relationship between pipe size, thickness and specimens, refer 6.2.5.2 for acceptance criteria, refer 9.3.5 for test frequency and other details.

On Sunday, October 8, 2017 at 4:22:33 PM UTC+5:30, BIJAYA GOUDA wrote:
Dear all,
I would like to inform that what are pipe sizes and thickness required impact test in API 5L PSL 2 as per API 5L standard.
Anybody knows about this, Please share the knowledge  about impact test.

Regards
Bijaya Gouda

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...