Tuesday, October 3, 2017

[MW:26860] Ferrite test

Dear experts

We have pipe SA 358 tp 304 CL 1
In EIL qap ferrite test is mentioned
How to check whether this test is really required. As per SA 358 it is supplementary requirement.
How FN to be decided for acceptance.  How to calculate.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...