Dear Mr Neilesh Kumar

Thanks for the quick response. I shall use it and in case of any doubt I will seek your advice.

Thanks and regards
N S Gurm

On 31-Aug-2017 11:54, "'Neilash Kumar' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Hi ,

Its good to see your mail subject regarding validation , There is separate clause in API SPEC Q1 & API 5LD Section 7.5.2

Here are some information that you need to maintain separate format for Welding process validation.

A- DETAILS OF EQUIPMENT USED FOR VALIDATION
The process equipment's used for the validation shall be proven capable of performing the task for which they were designated

B- QUALIFICATION OF PERSONNEL INVOLVE IN THE VALIDATION
Welding Engineer / QC engineer shall ensure that only qualified personnel are assigned for the respective process, includes the weld overlay operator qualification

C- CRITERIA FOR REVIEW AND APPROVAL OF THE PROCESSS
Criteria for review and approval of the process shall be based on the criteria requirement specified in the appropriate qualification code and standard.

D-USE OF SPECIFIC METHOD AND PROCEDURES
WPS, PQR, Materials used, code requirements, specifications, procedures, inspection and testing, defining the acceotance criteria and its reference documents

E- REQUIREMENTS OF RECORDS
Equipment Operation Manual
Maintenance Records of Equipment
Calibration records for control pannel
Qualified WPS & PQR records
Operators Qualification records
Inspection & Testing records


Hope this clarifies your query and proceed further.

NEILASHKUMAR.P
WELDING ENGINEER


On Thursday, 31 August 2017 9:06 AM, Nachhattar Singh <nachhattar1947@gmail.com> wrote:


Dear Experts
 
I am required to submit to the client as to how the "VALIDATION OF THE WELDING PROCESS FOR
THE HARD FACING AND SEAT RING WELDING OF THE GATE VALVES" will be done. Following has already
Been complied and submitted but the client wants some more to be done:-
 
01.   WPS is accepted as submitted.
02.   PQR based on the WPS is in place and accepted.
03.   Heat treatment is not the requirement.
 
Please advise what else should be done, give the reference of such requirements.
 
Thanks in advance
 
NS Gurm
 
PLEASE THINK BEFORE PRINTING
 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...