Re: [MW:26763] CALRIFICATION FOR THE DEFECT

Dear Patel,


Above punch mark  Intrusions of foreign material during rollings and below punch mark lamination 

Regards,
Kishor

On Sun, Aug 27, 2017 at 6:38 AM, Patel Vivek <vivekpatel1303@gmail.com> wrote:
It's cold lap ...which is common defect during forging.....

On 26-Aug-2017 6:25 PM, "Shanmugam" <nss2410@gmail.com> wrote:
Dear Friends,
                       Can you identity the type of defect which was found in one of the material in our project during blasting.

With Regards,
N.Shanmugam

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...