Wednesday, August 23, 2017

Re: [MW:26745] valve flow direction

There's no issues. 

Best regards 

P.VENKATESH 



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: Rameez khan RK <rk.rameezkhan21@gmail.com>
Date: 21/08/2017 23:02 (GMT+05:30)
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:26737] valve flow direction

Dear Expat,
                       I have a question regarding gate valve flow direction. if the direction change during fit up then what type of problem facing can any one tell me regarding this issue. 



Thanking you

Rameez khan 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...