Saturday, August 19, 2017

Re: [MW:26729] WPS/PQR using within group

Dear Mr. Mubeen,

Following Para of ASME Sec. IX 2017

QG-106.1 Procedure Qualifications.
(c) If the effective operational control of procedure
qualifications for two or more companies of different
names exists under the same corporate ownership, the
companies involved shall describe in their Quality Control
System or Quality Assurance Program the operational
control of procedure qualifications. In this case, separate
procedure qualifications are not required, provided all
other requirements of this Section are met.

Regards,

Muhammad Babur Khan Lashari
Sr. QA/QC Inspector

(CSWIP 3.1 / CWI II From PWI) 

 Khaled Juffali Industrial Company

Mob: + 966 56 2179280 / 58 2774568

PAK : + 92 334 6186285

Skype: babur.lashari

E-Mail: babur.khan@kjgroup.com


On Tue, Aug 8, 2017 at 5:40 AM, mubeen mubeen <mubeenaws@gmail.com> wrote:
Good Day all,

Please help me out to locate clause in ASME IX for using sister company/group company qualified WPS with other company(same group)after their Welders qualification.Also provide guidance is there any mandatory requirement to include such clause details in QMS or document control procedure?

Thanks & regards,
Mubeen

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...