Re: [MW:26707] interpass temperature

Hi,

Refer para 8.0 and Table 4 of API RP 582-2009.

On Sat, Aug 5, 2017 at 5:44 PM, TDK YOKESH <tdky167@gmail.com> wrote:
> Hello sir ,
>
> Generally the minium interpass temp is your preheat temp . Preheat temp can
> be calculate as per BS EN 1011-2 .
>
> On 2 Aug 2017 6:52 a.m., "samaran sadasivam" <ssamaran@gmail.com> wrote:
>>
>> Dear Experts,
>>
>>
>> Where should I refer the inter pass temperature values as per material
>> wise or P.no wise
>>
>> Is there any guidelines for inter pass temperature??
>>
>> I have seen ASME B31.3 T330.1.1 notes mentioned below but its not enough.
>>
>>
>> Thanks & Regards
>>
>> S.Samaran
>> +91 9486664977
>>
>> --
>> https://materials-welding.blogspot.com/
>> https://www.linkedin.com/groups/122787
>> ---
>> You received this message because you are subscribed to the Google Groups
>> "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an
>> email to materials-welding+unsubscribe@googlegroups.com.
>> Visit this group at https://groups.google.com/group/materials-welding.
>> For more options, visit https://groups.google.com/d/optout.
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.



--
Thanks, & With Best Regards,



Dharmesh MISTRY

+91 9820735814

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.