Re: [MW:26705] Welding of Alloy800 # SA 213 T11

U can go ER NiCrFe6 also

On 05-Aug-2017 9:21 PM, "PREM SHANKARDUTT NAUTIYAL" <prem_nautiyal@rediffmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (prem_nautiyal@rediffmail.com) Add cleanup rule | More info

Dear Friends

A heat exchanger is being fabricated as per ASME Sec VIII Div.1.

Service Temp is @ 480 degree C.

Tubes material is SA 213 T11 - 1Cr,0.5Mo.

Tube sheet material is SB 409 (Alloy 800)- 33Ni, 42Fe,21Cr UNS No. N08800.

We have selected TIG filler as ER NiCr-3 for the tube to tubesheet joint.

Is the selection of filler metal satisfactory or any better alternative ?

Regards

Prem Nautiyal
cell: 9769316004


PREM S NAUTIYAL
CELL : 9769316004

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...