Re: [MW:26702] interpass temperature

Hello sir , 

Generally the minium interpass temp is your preheat temp . Preheat temp can be calculate as per BS EN 1011-2 . 

On 2 Aug 2017 6:52 a.m., "samaran sadasivam" <ssamaran@gmail.com> wrote:
Dear Experts,


Where should I refer the inter pass temperature values as per material wise or P.no wise

Is there any guidelines for inter pass temperature??

I have seen ASME B31.3 T330.1.1 notes mentioned below but its not enough. 


Thanks & Regards

S.Samaran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...