Dear Mr Vijay Katkar,

Supplementary essential variable comes into effect only when toughness requirement is specified, Since in your case it is not required, ASME gives the flexibility to use the same WPS/PQR for single wire/three wire combo SAW process (Refer QW 410.10).

Regards,
Bala Guru Nathan C,
QA/QC Engineer, L&T Construction.

On Tuesday, June 6, 2017 at 12:50:25 PM UTC+5:30, vijay Katkar wrote:

Dear All,          

 

Need your help.

 

I have SAW process PQR with three wire combination, Can I use this PQR with single wire ?

 

Equipment is not required Impact test.

 

Change from Single to multi electrode and vice versa  is a supplementary essential variable.

Current & Polarity of these wires are DCEP.


Is there any other variable which restrict to use multi-electrode to single?  please guide me on this.

 

Regards 


Vijay Katkar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...