Hi,

As far as the essential variables(ASME Sec IX) and specific client/project requirements are satisfied in your WPS/WPQT, ASME gives you the flexibility to use the same for different projects.

But in some cases, the client will ask you to qualify the welders(WPQT) & procedure(WPS/PQR) in presence of an inspection authority/Client representative, so in those situations you have to prepare new documents.


Regards,
Bala.

On Wednesday, August 23, 2017 at 6:10:43 PM UTC+5:30, asif.raza wrote:

Dear Experts

 

Pl let me know as per ASME, is it possible to use some others project PQR in other project as develop WPS, or we have to have first pWPS, WPS and PQR through our qualified welders…. Pl do share code/standards as possible.

 

Thanks

 

Raz Khan

 

 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...