Wednesday, August 23, 2017

[MW:26743] OXY - ACETYLENE Gas cutting in lethal service piping.

Dear Experts,

 

We have 3" Dia piping 15 mm Thickness CS material used for lethal service piping. Due to site modifications the pre welded pipe and fittings has to be cut and re welded. Is OXY - ACETYLENE Gas cutting allowed for cutting the piping?

 

After cutting, bevel preparation has carried out by grinding by cutoff wheel.

 

Regards

V.Kingsly Geo.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...