-- Please give the advise below mentioned PQRs supporting to the WPS
WPS
1. Thickness range (Groove) : 6.02 mm to 21.94 mm (Process GTAW+SMAW)
PQRs
1. Thickness of the test coupon is 6.02 mm (Process GTAW+SMAW)
2. Thickness of the test coupon is 10.97 mm (Process GTAW+SMAW)