Grinding does not affect material after pwht as temp are too low. Grinding is done for removing thermo couples all the time. Even temporary supports are cut and ground after pwht.

Rgds
Prakash. G.
Independent Consultant. ASME/ISO
From: Umar Makrani
Sent: Saturday, 27 December 2014 07:58
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: Re: [MW:22651] Grinding of weld joints after PWHT

I think no. My belief is reinforced by sometimes we replace the pwht with temperbead in which we grind the half bead. Expect views from other experts. 

 

 

Thanks & Regards

 

Firoz Ahmed R. Makrani, PMP®

Sr. Inspection Engineer

Description: safety_head_600X90_velosi its comingOn 26 Dec 2014, at 13:03, Ali Al-Zawamri <alzawamri@gmail.com> wrote:


Dear,

Grinding afte PWHT may create or hardning the weld joint.  So it is better to do before PWHT.
waiting for the team input.

Thanks,

On 26 Dec 2014 10:50, "Vikas Sahu" <viksahu@gmail.com> wrote:
Dear sir,
              Please give reference /code/standard/writeup for Grinding (upto what extent) permitted or not after PWHT of Weld Joints of piping.

Regards
Vikas sahu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...