RE: [MW:22649] Grinding of weld joints after PWHT

PWHT is the last activity, and after weldingworks completion, hence no meaning doing grinding after PWHT.

Lakshman kumar.B
Project manager.
9440031459

From: Ali Al-Zawamri
Sent: ‎26-‎12-‎2014 20:24
To: materials-welding@googlegroups.com
Subject: Re: [MW:22647] Grinding of weld joints after PWHT

Dear,

Grinding afte PWHT may create or hardning the weld joint.  So it is better to do before PWHT.
waiting for the team input.

Thanks,

On 26 Dec 2014 10:50, "Vikas Sahu" <viksahu@gmail.com> wrote:
Dear sir,
              Please give reference /code/standard/writeup for Grinding (upto what extent) permitted or not after PWHT of Weld Joints of piping.

Regards
Vikas sahu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...