Wednesday, December 24, 2014

RE: [MW:22628] Positive Material identification (PMI)

Just simply use the magnet to check weld root and cap whether magnetic or non-magnetic which will differentiate CS and SS.

 

 

Rgds,

 

Win Naing

Senior Inspection Engineer

Inspection and Corrosion Dept.

TOTAL E&P MYANMAR

Office  : 00 95 (1)  650 977, 650 989, 660 466 Ext 3328

Mobile: +95 9 5138585

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Zakaria ghrab
Sent: Tuesday, December 23, 2014 11:19 PM
To: materials-welding@googlegroups.com
Subject: [MW:22627] Positive Material identification (PMI)

 

Dear all,

 

  Could you please help us.

 

In our project, austenitic stainless steels welds, we have a doubt for some welds that may be welder used GTAW carbone steel filler metal in root pass.

 

We propose to use PMI inspection but we're not sure about result fiability (root CS + Cap/Filling SS).

 

Regards.

-----

GHRAB Zakaria

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...