Friday, March 28, 2014

Re: [MW:20422] Qualification thickness range for welder test

Ranges
1. Dia  -----   From 73 mm OD to Unlimited
2. Thickness ------ 2 times deposited thickness for each process. OR 
3. if any of the process means GTAW OR SMAW weld deposited with a minimum three layesr and atleast 13 mm thick weld deposited qualification will be maximum.

Thanks
Regards
Intekhab Alam Ansari



On Thu, Mar 27, 2014 at 9:22 AM, Apurba Mazumder <apurba123.duet@gmail.com> wrote:
Dear Sir,
I have taken welder test on 6" pipe at 21mm thickness , parent material specification is ASTM A 672 GR C65, Group no 1 to Group 1. Filler material specification ER70S-6,& E8018 C1.Can you inform me, What will be the qualification thickness range for this test.

Best regards

Apurba Mazumder
QA & QC Engineer
The Pileline Engineers & Associates Ltd.
Bangladesh.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...