Tuesday, March 25, 2014

Re: [MW:20408] PWHT AS PER ASME SEC-I

Hi,
It clearly states that as :Nominal thickness of Weld" It means the weld deposit/thickness. 
In your case its a Set-on type and weld deposit/thickness is 12mm only. So no need to do PWHT. 
 
Thanks & Regards,

(Karthik)

Karthikeyan.S
QA/QC Manager
German-Thai Boiler Engineering Cooperation Limited.
Rayong Factory ;
379 Moo.6 Soi 8, Tambol Pananikom,
Nikompattana, Rayong 21180 THAILAND
Tel : +66 38 897 035-9 Ext. 137
Fax : +66 38 897 034
Hand Phone: 0066 892512282


On Saturday, March 22, 2014 7:49 PM, "rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA" <rajesh.mhaske17@gmail.com> wrote:
Dear sir
          ASME SEC-I ,PW-39
2)when the nominal thickness of a weld as defined in PW-39.4 is greater than % in. (19 mm) but does not exceed 1 % in. (38 mm), and:
(a) the calculated carbon equivalent, CE, of any of the basemetals in the weld joint is less than or equal to 0.45, using the formula :
                               CE = C + (Mn + Si)/6 + (Cr + Mo v)/S + (Ni + CU)/15
Can I use above clause of ASME SEC-I ,PW-39 to following welding to eliminate the PWHT of  membrane panel header
  1. Item : Membrane Panel
  2. Material : SA106 Gr B and SA210 Gr A1
  3. OD and thk : 273 *35 header,panel tube : 50.8*6.35 thk
  4. Joint type : Groove +Fillet
  5. Weld deposition : 12 mm
  6. No of Tube : 35 nos
  7. CE : less than 0.45
  8. preheat : 100 deg C
  9. boiler type : CFBC
  plz suggest
Regards
Rajesh S Mhaske
Engineer Welding,CSWIP3.1,ASNT Level-II
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...