Re: [MW:20398] Re: Requirment of Hardness Test for PQR of SB 575 UNS N06059.

ASME has no requirement.
VDM alloy 59 is a Ni-base alloy and normally, there are no hardness requirements for FCC alloys (full austenite or Ni-base) unless they are to be used at low temp service (Cryogenic service).

Regards
Ramin Kondori
Sr. QA/QC Engineer
SINOPEC

r.kondori@petroyada.com
+98-2123592322
+98-9132150320



On Sat, Mar 22, 2014 at 9:30 AM, kannayeram gnanapandithan <kgpandithan@gmail.com> wrote:
no requirement

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Fri, Mar 21, 2014 at 3:36 PM, rajesh s. mhaske ,Engineer Welding ,PUNE,INDIA <rajesh.mhaske17@gmail.com> wrote:
Dear Ganesh sir,
  Hardness values are dependent upon factors such as alloy content, weld preheat and postweld heat treatment. Specific hardness test for welded joints are not specified in asme sec -ix except Temper bead and overlay .

in your case hardness test is not required for low carbon  nickel-chromium-molybdenum-copper alloy steel
but it is also defend upon specification of  your customer ,design application or  service application so refer your  specification of customer

Rajesh S Mhaske
Engineer Welding
CSWIP 3.1,ASNT Level-II




On Thursday, March 20, 2014 10:49:24 PM UTC+5:30, Ganesh Mahankal wrote:
 
Dear All,
 
While performing a PQR of butt joint (plate to plate ) of SB 575 UNS N06059 to SB 575 UNS N06059 with ASME sec IX ,
Is it a hardness test is required ? ( except tension & bend ).
Is this hardness requirement is requirement of other code like Sec II part B?
 
plz guide.
 
Ganesh Mahankal
Alfa Laval India Ltd Pune India
+91 9970357971
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon