Friday, March 21, 2014

Re: [MW:20393] Tack welding

Is that a tack weld which is going to remain on place?
If not, you need neither a qualified WPS nor a qualified welder
refer article 4 sectionIX fillet qualification table


On Thu, Mar 20, 2014 at 2:17 PM, Vikas Sahu <viksahu@gmail.com> wrote:

Yes , tack welding can be done,refer article 4 sectionIX fillet qualification table

On 19-Mar-2014 5:59 PM, "mahammed javeed" <javeedcwi@gmail.com> wrote:
Gentle men,

My question regards to the tack welding. I have to make a  bridge tack weld on a 2" SS pipe. As per my company procedure tack welding shall be done by a qualified welder with a qualified procedure. 

As per my knowledge bridge tack is a fillet weld and if a welder is qualified on 6G position on a pipe he is qualified to do so. 

The problem with my client is he said the procedure is not qualified as the base metal thickness qualified for the WPS is 1.5mm to 8.4 mm and the actual base metal thickness is 8.7mm. 

As it is a fillet weld I think the WPS is qualified for tack welding also

Hope to get your clarification on this subject.

Best Regards
M. Javeed

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--

sushil gaur

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...