QW-301.2, 2nd paragraph,  “The weldor or welding operator who prepares the WPS qualification test coupons meeting the requirements of QW-200 is also qualified within the limits of performance qualifications listed in QW-304 for welders and in QW-305 for welding operators.  He is qualified only within the limits for positions specified in QW-303.”

 

Obviously, in such case, the weldor/welding operator is not working to a qualified WPS.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of mahammed javeed
Sent: Tuesday, March 18, 2014 9:40 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:20378] RE: 20357] Re: Welder Qualification

 

Any reference that for the WQT of test plate doesn't require a WPS  ?

 

Regards

Javeed

 

On Tue, Mar 18, 2014 at 5:12 PM, John Henning <jhenning@deltak.com> wrote:

Only exception is for a weldor performing the procedure qualification test plate welding.  He would be qualified while welding without a qualified WPS in hand.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of rajesh mhaske ,Welding Engineer
Sent: Tuesday, March 18, 2014 4:16 AM
To: materials-welding@googlegroups.com
Subject: [MW:20357] Re: Welder Qualification

 

Is a WPS is required for conducting WQT  :ANS : YES, WPS is req during the WQT
can we use a preliminary WQT  : ANS : NO
The WPSs shall be identical for all the essential variables, except for the
preheat temperature and PWHT requirements. or has an SWPS
adopted in accordance with Article V,ASME SEC-IX


On Sunday, March 16, 2014 10:23:06 AM UTC+5:30, mahammed javeed wrote:

Gentle men,

 

My question is regarding to the welders qualification test, My client is insisting to use a qualified WPS for qualification of WQT, Is a WPS is required for conducting WQT? or can we use a preliminary WQT or just follow the essential varialbles list as per ASME Sec IX?

 

Regards

M. Javeed

Quality supervisor

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...