Re: [MW:20374] WPQ COMBINATION

 Dear Rajesh,
As per My Knowledge
No, 
Because, 
Your welder A cannot weld below 73 mm OD.
Also both of your welder cannot deposit maximum because during initial qualification they not deposit at least 13 mm with  three layers  to qualify for maximum deposition.
Thanks
Regards
Ansari


Thanks
Regards
Intekhab Alam Ansari



On Tue, Mar 18, 2014 at 5:02 PM, rajesh mhaske ,Welding Engineer,PUNE <rajesh.mhaske17@gmail.com> wrote:
Welder A:
First WPQ
Qualification test coupon: 168 OD X 18.26 mm
Welding Process: GTAW + SMAW
Deposition Qualn Range: GTAW = 8 mm, SMAW = Max to be welded.
Welding Position: 5G
Position Qualn Range: F, V, O

Second WPQ
Qualification test coupon: 63.5 OD X 6.35 mm
Welding Process: GTAW + SMAW
Deposition Qualn Range: GTAW = 4 mm, SMAW = 8.7.
Welding Position: 6G
Position Qualn Range: All

Welder qualification as per ASME sec IX

Can these two qualifications be combined as below:
Qualification min OD: 25 mm
Welding Process: GTAW + SMAW
Deposition Qualn Range: GTAW = 8 mm, SMAW = Max to be welded.
Position Qualn Range: All

Please suggest.

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...