Wednesday, March 19, 2014

Re: [MW:20371] WPQ COMBINATION

Hi rajesh

yes

but consider F No,BACKING,BASE MATERIAL ,GTAW polarity and purging gas also.

Regards
R.Prabhakaran


On Tue, Mar 18, 2014 at 5:02 PM, rajesh mhaske ,Welding Engineer,PUNE <rajesh.mhaske17@gmail.com> wrote:
Welder A:
First WPQ
Qualification test coupon: 168 OD X 18.26 mm
Welding Process: GTAW + SMAW
Deposition Qualn Range: GTAW = 8 mm, SMAW = Max to be welded.
Welding Position: 5G
Position Qualn Range: F, V, O

Second WPQ
Qualification test coupon: 63.5 OD X 6.35 mm
Welding Process: GTAW + SMAW
Deposition Qualn Range: GTAW = 4 mm, SMAW = 8.7.
Welding Position: 6G
Position Qualn Range: All

Welder qualification as per ASME sec IX

Can these two qualifications be combined as below:
Qualification min OD: 25 mm
Welding Process: GTAW + SMAW
Deposition Qualn Range: GTAW = 8 mm, SMAW = Max to be welded.
Position Qualn Range: All

Please suggest.

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...