Dear Santhosh,

Thanks for the reply,

 As Contractor, we have inform the supplier and Sub contractor to follow the standard of color coding for material identification. While shipping or fabrication time if they mix up material like P91,P22, P11 etc it will be a problem for us. I have a book (Pipe Fabricators Textbook, American standard 1999 version. In that only mentioned CS,SS etc not for Alloy like P91,22,11 etc. If any one have these with latest version please share with me.


Thanks n Regards

Arun


On 18 March 2014 11:13, SANTOSH K <subject.related@gmail.com> wrote:
Dear Arun,

There is no standard color coding from ASME/ASTM. If you go through ASME Sec - II says ( SA-106/SA-106M ) purchaser has to specify the color coding.

Any how refer  BS 5383 Specification for material identification of steel, nickel alloy and titanium alloy tubes by continuous character marking and colour coding of steel tubes, You may get some information.

Check with your client if they are having any specification for the same or propose any colors in your color coding procedure.

Regards,
Hema Santosh.



On Mon, Mar 17, 2014 at 5:07 PM, Arun Kumar.P <arun.ehr@gmail.com> wrote:
Dear Experts,

  Kindly provide me the standard for colour coding of pipe material (P91,P22,P11, Carbon Steel) also colour for each meterial identification.


Thanks and Regards

Arun

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...