RE: [MW:20369] Re: GTAW Filler Metal with a "G" suffix in ASME Sect. IX

In lieu of A-No. , the WPS will be limited to weld metal composition or Brand and Type of filler metal. 

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george.dilintas@gr.bureauveritas.com
Sent: Monday, March 17, 2014 12:53 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:20362] Re: GTAW Filler Metal with a "G" suffix in ASME Sect. IX

 

Check what is written in QW 404.5

In lieu of an ANumber designation, the nominal chemical
composition of the weld deposit shall be indicated on
the WPS and on the PQR. Designation of nominal chemical
composition may also be by reference to the AWS classification
except for the "G" suffix classification, the manufacturer's
trade designation, or other establ ished
procurement documents.

Consider also this explanation:

This specification includes filler metals classified
as R(X)XX-G [RMXX-G]. The "G" indicates that
the filler metal is of a general classification. It is general
because not all of the particular requirements specified
for each of the other classifications are specified for this
classification. The intent in establishing this classification
is to provide a means by which filler metals that differ in
one respect or another (chemical composition, for example)
from all other classifications (meaning that the composition
of the filler metal, in the case of the example, does not
meet the composition specified for any of the classifications
in the specification) can still be classified according to the
specification. The purpose is to allow a useful filler metal—
one that otherwise would have to await a revision of the
specification — to be classified immediately under the
existing specification. This means, then, that two filler
metals, each bearing the same "G" classification, may be
quite different in some certain respect (chemical composition,
again, for example).
 
Conclusion: do not use a "G" filler metal to qualify a WPS. You will be in trouble with the A - No



best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS

Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
(See attached file: Dilintas_George.vcf)


krishnasamy1968 ---14/03/2014 06:13:46---Customer Sent from Samsung Mobile

From: krishnasamy1968 <krishnasamy1968@hotmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: 14/03/2014 06:13
Subject: Re: [MW:20322] Re: GTAW Filler Metal with a "G" suffix in ASME Sect. IX
Sent by: materials-welding@googlegroups.com





Customer


Sent from Samsung Mobile


-------- Original message --------
From: kannayeram gnanapandithan
Date:13/03/2014 1:42 PM (GMT+03:00)
To: materials-welding
Subject: Re: [MW:20310] Re: GTAW Filler Metal with a "G" suffix in ASME Sect. IX

Who is purchaser? Manufacturer or Customer?

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Wed, Mar 12, 2014 at 3:12 PM, KRISHNASAMY MASANAM <krishnasamy1968@hotmail.com> wrote:

No, required as per ASME Sec II C SFA-5.18 Table 1, Table 3, kindly find the attached files for your references...

     

Thanks & Best regards

 

Krishnasamy. M

Mechanical/Welding Inspector

Saudi Aramco Project Inspection Department

TUV NORD - KSA

krishnasamy.masanam@aramco.com 

KSA +966 564743358 (Available)

INDIA +91 9442558057

 


Date: Wed, 12 Mar 2014 10:31:37 +0530
Subject: Re: [MW:20295] Re: GTAW Filler Metal with a "G" suffix in ASME Sect. IX
From: kgpandithan@gmail.com
To: materials-welding@googlegroups.com

not required

THANKS & BEST REGARDS
KG.PANDITHAN, AWS-CWI, CSWIP 3.1
CONSULTANT-WELDING & QUALITY


On Tue, Mar 11, 2014 at 2:15 PM, KRISHNASAMY MASANAM <krishnasamy1968@hotmail.com> wrote:

Dear all,
                       If you are using those electrodes it shall be approved from the owner/client, its mandatory requirement as per ASME Sec II C

     

Thanks & Best regards

Krishnasamy. M
Mechanical/Welding Inspector
Saudi Aramco Project Inspection Department

TUV NORD - KSA
krishnasamy.masanam@aramco.com 

KSA +966 564743358 (Available)

INDIA +91 9442558057




Date: Mon, 10 Mar 2014 22:40:18 +0530
Subject: Re: [MW:20286] Re: GTAW Filler Metal with a "G" suffix in ASME Sect. IX
From: ranendrac6@gmail.com
To: materials-welding@googlegroups.com

I am just adding one thing. Suffix G means general and it can be any combination. If anybody wants to purchase Electrode/Filler with suffix G,then he needs to specify the correct combination to avoid any last minute confusion.

Regards,
Ranendra


On Mon, Mar 10, 2014 at 11:16 AM, Ramin Kondori <raminkondori@gmail.com> wrote:

Dear Mr. Rezazade:

Be careful when using filler metals with a "G" suffix since they may have any combination of alloying elements and only by referring to manufacturer catalogue you can find out which alloying element(s) they have used.

Once I remember that a company qualified a WPS with E8018-G (that later I found it had Cr/Mo additions) and during production their procurement officer purchased another E8018-G (that later I found it had Nickel additions).
This caused the company a lot of trouble since these are two different filler metals with different properties. Ni additions are suitable for low temp service but Cr/Mo additions improves high temp service properties (the application was a gas turbine exhaust - high temp service).

So always check the catalogue before proceeding with PQR or production.

Ramin Kondori
Sr. QA/QC Engineer
SINOPEC

r.kondori@petroyada.com
+98-2123592322
+98-9132150320



On Sun, Mar 9, 2014 at 4:08 PM, M Rezazade <inspectormag@gmail.com> wrote:

 Dear sir
QW-404.12 is supplementary essential variable and when impact test required in your WPS (or production) according to construction code, you need to consider it as essential variable.
 .so changing the brand of G suffix electrode is not permitted in WPS without re qualification of PQR with new brand of electrode. (when impact test required)

در سه‌شنبه 9 فوریهٔ 2010، ساعت 5:10:20 (UTC+3:30)، yan نوشته:

Hi Gentlement,
We have many qualified  WPS/PQR (GTAW process) using filler metal with a "G" suffix such as ER-70S-G and qualified base on ASME Section IX ( using previous ASME IX  Ed. 2004/Ed. 2007) . In QW-404 / Filler Metals), para QW-404.12  state that change classification is NON ESSENTIAL VARIABLE. But in ASME IX Ed. 2007 addendum 2008, in the same QW-404.12 state that change in classification is SUPPLEMENTARY ESSENTIAL VARIABLE ( a filler metal with a" G" suffix)Our question is  whether this existing WPS/PQR need re-qualification (change from NON ESSENTIAL VAR to SUPPLEMENTARY ESSENTIAL VAR)?
Great thank to get sharing accordingly.
Regards,
Yan
Powered by Telkomsel BlackBerry®


--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.



--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...