Monday, March 17, 2014

RE: [MW:20363] Combination of welding procedures

BEGIN:VCARD
X-LOTUS-CHARSET:UTF-8
VERSION:3.0
PRODID:-//Lotus Development Corporation//NONSGML Notes 8.5.2//EN_C
FN:George H Dilintas/GRC/VERITAS
N:Dilintas;George;;;
ADR;TYPE=WORK;TYPE=PREF:PIRAEUS;;23\, Etolikoy Str.;PIRAEUS;;185 45
;GREECE
ADR;TYPE=HOME;TYPE=PREF:;;19-21 B. Laskou str.;Athens;Attika;11 633
;Greece
TEL;TYPE=HOME:+30-1-7667 197
TEL;TYPE=WORK:+30-210-40 63 113
TEL;TYPE=HOME;TYPE=FAX:+30 - 1 - 7667 197
TEL;TYPE=WORK;TYPE=FAX:+30-210-40 63 118
TEL;TYPE=CELL:+30 -69 44-64 62 04
EMAIL;TYPE=WORK;TYPE=PREF;TYPE=INTERNET
:george.dilintas@gr.bureauveritas.com
ORG:Bureau Veritas;Industry
REV:20131201T024559Z
END:VCARD

I do not think that you can.
Two essential variables do not match (process and T)

    best regards

    Dr. Georgios Dilintas

    Authorized Nuclear Inspector
    Authorized Inspector Supervisor
    API 510 Inspector

    I&F REGIONAL TECHNICAL MANAGER
    BUREAU VERITAS HELLAS

    Tel: +30 210 40 63 113/4
    Fax: +30 210 40 63 118
    Cell: +30 69 44 64 62 04
    (See attached file: Dilintas_George.vcf)

"John Henning" ---17/03/2014 16:20:18---I presume that you asking about base meal thickness.

From: "John Henning" <jhenning@deltak.com>
To: <materials-welding@googlegroups.com>
Date: 17/03/2014 16:20
Subject: RE: [MW:20352] Combination of welding procedures
Sent by: materials-welding@googlegroups.com




I presume that you asking about base meal thickness.
 
While they can be combined, the minimum thickness for the combined procedure is 5mm (assuming you are not going to separate by process).  FCAW cannot be used on any thickness below 5mm, therefore if you use a single value for minimum thickness on the WPS, the limiting minimum thickness  is that for the FCAW.  If all other essential variables the same for GTAW, you could use the two PQRs for a single WPS qualified from 1.5mm to 200mm.  And a second WPS for FCAW qualified 5mm to 200mm.  To bring the qualified FCAW thickness you need a PQR qualified on thickness < 10mm.
 
John A. Henning
Welding & Materials
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Dhamodaran
Sent:
 Sunday, March 16, 2014 4:06 AM
To:
 materials-welding@googlegroups.com
Subject:
 Re: [MW:20342] Combination of welding procedures
 
Dear Vishal,
 
Yes it can be combined,Plz. refer QW-200.2(f).
 
Regards
Dhamodaran
 
On Sunday, 16 March 2014 11:03 AM, Vishal Chakote <chakotevishal47@gmail.com> wrote:
Combination of welding procedures.

PQR-A:
Welding Process-GTAW
Material - P-No.1 to P-No. 4
Qualn Range - 1.5-10mm

PQR-B:
Welding Process-GTAW+SMAW+FCAW
Material - P-No.1 to P-No. 4
Qualn Range - 5 - 200mm

Can these PQR's be combined for new WPS for
Welding Process - GTAW+FCAW
Material - P-No.1 to P-No. 4
Qualn Range -
1.5  5-200mm.

The above WPS's are made according to the ASME sec IX.
Give your suggestion.

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.
 
--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...