RE: [MW:20355] Acceptable Values for Charpy Impact Test at -(minus) 196 degC for A312 TP304

Problem is they never tell us the whole story.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of george.dilintas@gr.bureauveritas.com
Sent: Monday, March 17, 2014 1:01 PM
To: materials-welding@googlegroups.com
Subject: RE: [MW:20353] Acceptable Values for Charpy Impact Test at -(minus) 196 degC for A312 TP304

 

Yes John.
However, for those who are using ASME for Pressure equipment to be certified in accordance with 97/23/EC, besides the lateral expansion, the value of 27 Joule has to be obtained on a standard ISO specimen

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor
API 510 Inspector

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS HELLAS

Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
(See attached file: Dilintas_George.vcf)


"John Henning" ---14/03/2014 17:05:06---For stainless steels in low temperature applications, charpy impact acceptance criteria is lateral e

From: "John Henning" <jhenning@deltak.com>
To: <materials-welding@googlegroups.com>
Date: 14/03/2014 17:05
Subject: RE: [MW:20329] Acceptable Values for Charpy Impact Test at -(minus) 196 degC for A312 TP304
Sent by: materials-welding@googlegroups.com





For stainless steels in low temperature applications, charpy impact acceptance criteria is lateral expansion not absorbed energy.  For example see ASME Sc. VIII UHA-51 or B31.3 paragraph 323.3.5(b).
 
John A. Henning
Welding & Materials
 
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Tri Yulianto
Sent:
 Friday, March 14, 2014 8:08 AM
To:
 materials-welding@googlegroups.com
Subject:
 Re: [MW:20328] Acceptable Values for Charpy Impact Test at -(minus) 196 degC for A312 TP304

 

Hi Choudhary,

Please see ASTM A 370 table 9 for charpy  value acceptance criteria for subsize specimen.

Cheers,

Tri Yulianto
BAM Clough JV - Wheatstone LNG
On Mar 14, 2014 8:00 PM, "Anurudh Choudhary" <theoilgasengineer@gmail.com> wrote:
Dear All,
 
I'm using A312 TP304 pipe for design temperature -(minus) 196 degC for BOIL OFF GAS (BOG) service.
 
we have carried out the charpy impact test at -(minus) 196 degC for the pipe. we are having average value of Joules for pipe specimens.
 
Please provide/guide me with the Acceptable value for Charpy impact values( Joules) at -(minus) 196 degC along with codes/reference for A312 TP304 Pipe.
 
Kind Regards,
 
Choudhary Anurudh
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...