Tuesday, March 18, 2014

Re: [MW:20352] What is NON DESTRUCTIVE ELECTRIC TEST

Dear freind,
There is a NDT called Eddy Current testing.
Check especially for pipes which suffices the Hydro test requirement....
regards,
Debasish


On 13 March 2014 04:51, B R Meghwal <br.meghwal@fernas.co.in> wrote:

Hi,

 
When i am passing through some of the ASTM materials standard, e.g A106 / A672 / A333...., i came through word NON DESTRUCTIVE ELECTRIC TEST, can any one define this What is NON DESTRUCTIVE ELECTRIC TEST, how can be differentiated from NDT & NON DESTRUCTIVE ELECTRIC TEST.

 

Your kind response will be highly appreciated.

 

Thanks & regards,

 

B.R.Meghwal
Dy. Manager-QA/QC

(ASNT Level 3,AWS-CWI & CSWIP3.1)

 

FERNAS Construction India Pvt. Ltd.

(A wholly owned Subsidiary of FERNAS Construction Company Inc., Turkey)

Cyber Terrace, 16th Floor, Tower – B, Building No. 5, DLF Cyber City, Phase – 3

Gurgaon – 122 002, Haryana, INDIA.

(: +91 124 4937984       (M) : +91 82380 75168

The easiest way to escape from the problem is to solve it.

https://encrypted-tbn0.gstatic.com/images?q=tbn:ANd9GcS9e4uXYXao0nRlOJhNEhHWSKDzeH2AxmeoTGx39Hd2tuwjL4k_TALütfen bu e-postayı yazdırmadan önce çevrenizi düşünün. Before printing this e-mail ask yourself: "Do I need a hard copy?"

 

Confidentiality Notice

This e-mail and the accompanying document(s) contain confidential information which is privileged and intended only for the addressee here of. If you are not the intended recipient, you are here by notified that any disclosure, copying, distribution or use of this e-mail and/or accompanying document(s) is strictly prohibited. If you have received this e-mail in error, please immediately notify the sender at the above e-mail address

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...