I presume that you asking about base meal thickness.

 

While they can be combined, the minimum thickness for the combined procedure is 5mm (assuming you are not going to separate by process).  FCAW cannot be used on any thickness below 5mm, therefore if you use a single value for minimum thickness on the WPS, the limiting minimum thickness  is that for the FCAW.  If all other essential variables the same for GTAW, you could use the two PQRs for a single WPS qualified from 1.5mm to 200mm.  And a second WPS for FCAW qualified 5mm to 200mm.  To bring the qualified FCAW thickness you need a PQR qualified on thickness < 10mm.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Dhamodaran
Sent: Sunday, March 16, 2014 4:06 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:20342] Combination of welding procedures

 

Dear Vishal,

 

Yes it can be combined,Plz. refer QW-200.2(f).

 

Regards

Dhamodaran

 

On Sunday, 16 March 2014 11:03 AM, Vishal Chakote <chakotevishal47@gmail.com> wrote:

Combination of welding procedures.

PQR-A:
Welding Process-GTAW
Material - P-No.1 to P-No. 4
Qualn Range - 1.5-10mm

PQR-B:
Welding Process-GTAW+SMAW+FCAW
Material - P-No.1 to P-No. 4
Qualn Range - 5 - 200mm

Can these PQR's be combined for new WPS for
Welding Process - GTAW+FCAW
Material - P-No.1 to P-No. 4
Qualn Range -
1.5  5-200mm.

The above WPS's are made according to the ASME sec IX.
Give your suggestion.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...