You can take the minimum thickness of 1.5 mm onwards.
 
 sridhar.

 


From: Vidhyapathi <vidhyapathi2020@gmail.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Sent: Sunday, 16 March 2014 2:34 AM
Subject: Re: [MW:20340] WQT Thickness Limits

Can weld 4mm, 
ASME now where mention min thick for welder qualification 

Regards, 

Vidhyapathi 

On 15 Mar, 2014, at 11:07 pm, Mask Man <z19081987@gmail.com> wrote:

Hai Experts,

       For WQT, as per ASME Sec IX QW 452.1 (b), up to 13mm thick qualified for 2t, above 13mm thick qualified for unlimited, but from the above what will be the minimum qualified thick.

For Example,

I qualified a wqt with 15mm, so now I qualified for unlimited thickness whether I can weld 4 mm wall thickness?

Regards,
Mask
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...