Saturday, March 1, 2014

Re: [MW:20202] ULTRA SONIC TESTING

Hi

The thumb rule for angle probe selection is (90degrees - bevel angle).

Regards  

Prem Nautiyal
9769316004


Sent from Samsung Mobile

mark89 <mayurkotiwar77@gmail.com> wrote:
Dear sir , 
 
As per my knowledge the thumb rule to select the probe angle is ( 90- t ) where t = thk of material . i would like to know how to select  probe angle in UT if material thk is more than 100 mm .

Thanks .
Regards , 
Mayur kotiwar 
mayurkotiwar77@gmail.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...