Monday, March 17, 2014

Re: Fw: [MW:20349] Sub : Radiography interpretations of Cement lined weld joints./FOR MORE WRITE

shiva,
there is nothing exclusive for cement lines piping, the parent construction code should be used.
 
Dear Engineers:
it would be great if you can post replies in smaller fonts, so the whole message can be read in single view, hope you understand.
cheers

On Sat, Mar 8, 2014 at 4:43 AM, sajidalam mohd. <engineer_makes_world@yahoo.co.in> wrote:

(1) API 1104 (WELDING OF PIPELINES AND RELATED FACILITIES).

(2) API 5L 45 edition SPECIFICATION /CODE FOR LINE PIPE.
 
Regards
Engr. Mohammad Sajid Alam  
Inspection Engineer
Saudi-Arabia
Mobile:-+966553043236
E-Mail:-engineer_makes_world@yahoo.co.in


On Thursday, 6 March 2014 3:04 PM, Sivashankar Nagamanickamsundaramoorthy <poovaishankar@yahoo.com> wrote:

Dear All,

Please provide reference documents / standards for the Radiography interpretations of the Cement lined CS pipe weld joints. Pl refer the attached drawing for the joint configuration details.


Regards

N.S.Sivashankar


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35763] Hardness range for CS+ Alloy0625 clad welding

Dear experts. I am currently in the process of qualifying a PQR for API 5L X65 + A350 LF6. Both material consists of a base metal with alloy...