Monday, March 31, 2014

[MW:20439] Premature Root bend failure of dissimilar strength materials


Gents,

Please share thoughts on this subject:-

Mat A :- API 5L X70
Mat B :- ASTM A105N
Process :- GMAW (STT)/FCAW
Dia:- 600NB
Thk :- 16.01mm for Pipe and 17.48 for Flange

Root bend Failure, Retests failed as well.

Regards.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...