[MW:20433] RE: 20432] Induction bend cutting during cross-country pipeline construction

The bends which are made with a pipe bending machine have to be to a much bigger radius of bend compared with an induction bend, which will be, for example 5D. Hence induction bends and site bends are used for very different purposes. If the design calls for an induction bend then that is what is required for geometry reasons. Normally induction bends are supplied with tangential ends and you weld to the tangential end, which is more round than the bent section. If you cut an induction bend you will find that it is more likely to be oval in cross-section. As a result welding fit-up can be bad and weld root defects can result. If good fit-up was achieved and the radiographs show no defects then I consider there is little basis for rejection, even if not exactly conventional.

 

Regards

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Saidur Rahman
Sent: 29 March 2014 15:15
To: materials-welding@googlegroups.com
Subject: [MW:20432] Induction bend cutting during cross-country pipeline construction

 

Dear Experts,

I am now working on a Ø30" cross-country pipeline project. At my project one AP(Angle Point) needed 12° Bend. so the fitter cut 22.5° induction bend in the middle & make it 11.25° & used it. I think that it is not acceptable. they should use pipe bending machine.

 

Experts comments needed & also applicable codes & standards regarding  field pipe bending.

Regards,

Md. Saidur Rahman

QA/QC

GTCL

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...