Wednesday, March 26, 2014

[MW:20416] RE: 20411] DSS vs SDSS welding.

dear sir,
i agree with weld.metal chemistry.

service is seawater line highly corrosive.


But as per ASME,there is same A number 8 is provided for both DSS n SDSS. And P.number also 10H and group also same 1.

its looks like a limitation of ASME or it is more libaral about metal classfication.

in what code or standard basis should i say to my construction for new WPS.

regards,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35754] interpration