[MW:20398] PWHT AS PER ASME SEC-I

Dear sir
          ASME SEC-I ,PW-39

2)when the nominal thickness of a weld as defined in PW-39.4 is greater than % in. (19 mm) but does not exceed 1 % in. (38 mm), and:

(a) the calculated carbon equivalent, CE, of any of the basemetals in the weld joint is less than or equal to 0.45, using the formula :

                               CE = C + (Mn + Si)/6 + (Cr + Mo v)/S + (Ni + CU)/15

Can I use above clause of ASME SEC-I ,PW-39 to following welding to eliminate the PWHT of  membrane panel header

  1. Item : Membrane Panel
  2. Material : SA106 Gr B and SA210 Gr A1
  3. OD and thk : 273 *35 header,panel tube : 50.8*6.35 thk
  4. Joint type : Groove +Fillet
  5. Weld deposition : 12 mm
  6. No of Tube : 35 nos
  7. CE : less than 0.45
  8. preheat : 100 deg C
  9. boiler type : CFBC

  plz suggest

Regards

Rajesh S Mhaske

Engineer Welding,CSWIP3.1,ASNT Level-II

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...